濟南彩鋼瓦翻新施工重點是要防銹,施工時建議要從防銹效果的角度去制定施工方案,只有這樣才能做出好的工程質(zhì)量來。
Jinan color steel tile renovation construction focuses on rust prevention. During construction, it is suggested to formulate the construction scheme from the perspective of rust prevention effect. Only in this way can we make good project quality.
在噴涂前,先要對整個彩鋼瓦屋面的基本情況做充分的了解,包括但不限于彩鋼瓦目前現(xiàn)狀,比如銹蝕程度如何?如果只是輕微銹蝕,那么可以噴涂一遍底漆一遍面漆或者直接使用底面合一彩鋼瓦翻新漆,如果銹蝕比較嚴重的我們還是建議一底兩面這樣施工更加保險些。
Before spraying, it is necessary to fully understand the basic situation of the whole color steel tile roof, including but not limited to the current situation of color steel tile, such as the degree of corrosion? If it is only slightly rusted, you can spray one primer and one finish paint or directly use the bottom one color steel tile renovation paint. If the corrosion is serious, we still suggest one bottom and two sides, which is safer.
這里我們要注意,如果你的彩鋼瓦雖然銹蝕不是很嚴重,但是彩鋼瓦材質(zhì)是鍍鋅板的,我們不建議使用底面合一漆。斯鼎有專門針對鍍鋅板、白鐵皮等材質(zhì)的彩鋼瓦翻新漆,因為這些材質(zhì)如果是使用普通漆或者是底面合一漆,漆膜牢度會不太好。
Here we should note that if your color steel tile is not seriously rusted, but the color steel tile is made of galvanized sheet, we do not recommend the use of bottom integrated paint. Siding has renovated paint for color steel tiles made of galvanized sheet, white iron sheet and other materials, because if these materials use ordinary paint or bottom integrated paint, the fastness of the paint film will be poor.
在施工時,打磨除銹這個工序不要省略掉,彩鋼瓦翻新打磨清理很重要在生銹處打磨時好處理到能露出金屬光澤為止。彩鋼瓦翻新施工使用經(jīng)自己改造過的彩鋼瓦翻新打磨機設備,這大大提高了施工質(zhì)量。如果存在鐵銹,那么其附著在表面并不是那么牢固,它會阻礙底漆與基材表面的結合,從而影響到漆膜牢度。
During construction, the process of grinding and derusting should not be omitted. The renovation, grinding and cleaning of color steel tile is very important. It is best to polish the rusty place until it can expose the metallic luster. The renovation of color steel tile uses the renovated grinding machine equipment of color steel tile, which greatly improves the construction quality. If there is rust, it is not so firmly attached to the surface, which will hinder the combination of primer and substrate surface, thus affecting the fastness of paint film.
濟南彩鋼瓦
具體在施工時,各工序要做到位,特別是在打磨清理環(huán)節(jié),要想獲得好的效果,絕對不能馬虎,因為要確保底漆與基材緊密的結合,使得漆膜牢固,很好的隔絕空氣,起到防銹的作用。下一道涂層要等到上一道涂層完全干透后再噴涂,如果沒干透,很可能會出現(xiàn)起泡現(xiàn)象,因為里面有水分。
During the construction, all processes should be done in place, especially in the grinding and cleaning process. In order to obtain good results, we must not be careless, because we should ensure the close combination of primer and substrate, so as to make the paint film firm, isolate the air and prevent rust. The next coating shall be sprayed after the previous coating is completely dry. If it is not completely dry, blistering is likely to occur because there is water in it.
有些人可能會在水性彩鋼瓦翻新漆里面加一些水進去,我們建議如果是由于過于粘稠,影響到了施工,那么可以加入少量的水,不要超過5%,水加過量了,這漆也就報廢了。
Some people may add some water into the water-based color steel tile renovation paint. We suggest that if it is too viscous and affects the construction, a small amount of water can be added, not more than 5%. If the water is added too much, the paint will be scrapped.
總之,彩鋼瓦翻新施工要因地制宜,然后是各個環(huán)節(jié)工序都做到位,做規(guī)范才算是標準施工。更多內(nèi)容就來關注我們的網(wǎng)站m.qianhairuiben.com咨詢了解吧!
In short, the renovation construction of color steel tiles should be adjusted to local conditions, and then all links and processes should be in place, and the standard construction is to make specifications. For more information, please visit our website m.qianhairuiben.com Com consultation to understand!